Polymer used |
Natural Rubber suitably blended |
Operation Temperature |
-10ºC to 70ºC |
Operational Atmosphere |
Heavy/Dusty/Sandy/Corrosive/Salty |
Operational Humidity |
0 to 100% |
Metal Parts Spec |
Seamless Steel Tube |
Properties of Elastomer |
|
Shore A Hardness |
55 to 65 |
Tensile Strength |
180 Kg/cm2 Minimum. |
Elongation at Break |
450% Minimum. |
Compression Set |
25% Max. |
Shear Bond Strength |
600 PSI / 42.18 Kg/cm2 |
After Heat Ageing |
|
Change in SH |
+5, -0 |
Change in TS |
±23% |
Change in EB |
+10%, -30% |
Compressive Load-Deflection Characteristics |
|
||||||||
Maximum compressive load carrying capacity |
17000 Kgs. |
||||||||
Minimum Torque Resistively |
5° on either side |